* The printer itself: Anycubic Photon Mono SE
* The printer itself: Anycubic Photon Mono SE
* A curing cookie box with UV light inside
* A curing cookie box with UV light inside
* A roll of toilet paper
* A small jar with isopropyl alcohol to wash prints
* A box with:
* A box with:
** bottles of resin (grey, transparent)
** bottles of resin (grey, transparent)
Line 18: Line 20:
** a silicon spatula to stir resin in the vat
** a silicon spatula to stir resin in the vat
** a syringe to measure resin
** a syringe to measure resin
** a brush to spread resin to make prints shiny


=== Experimental ===
=== Experimental ===
This printer is currently in the experimental state. Please don't use it without first talking to someone who has some experience.
This printer is currently in the experimental state. Please don't use it without first talking to someone who has some experience.


== Safety ==
== Precautions ==
Read this before starting.
 
=== Safety ===
Using the printer involves dangerous chemicals and processes:
Using the printer involves dangerous chemicals and processes:


* the resin is a skin irritant - always wear gloves and glasses
* the resin is a skin irritant - wear gloves and glasses. Always wash your hands after handling objects in the printer station.
* the resin stinks and can't be healthy - turn on the ventillation pipe
* the resin stinks and can't be healthy - make sure there's enough ventillation (there's a pipe in the wash room)
* isopropyl alcohol for cleaning is an irritant and stinky
* isopropyl alcohol for cleaning is an irritant and stinky
* the printer emits UV light, which leaks outside and [https://www.nature.com/articles/s41598-018-30738-6?error=cookies_not_supported&code=d80aa4b6-92fd-481b-915c-bddcd98eab3b damages] living organisms - rather be outside the room when it's working
* the printer emits near-UV light, which leaks outside and [https://www.nature.com/articles/s41598-018-30738-6?error=cookies_not_supported&code=d80aa4b6-92fd-481b-915c-bddcd98eab3b damages] living organisms - rather be outside the room when it's working
* drop used toilet paper in the chemical waste bucket on the floor
 
=== Cleanliness ===
Resin is sensitive to sunlight (405nm wavelength) and hardens after a day or so even in the relative dark.
 
* Wipe resin from surfaces using toilet paper when you leave the station.
* Use brown containers to store extra resin
* After using a brush or syringe or some other tool with resin, wash it well with isopropyl alcohol.
 
=== Materials ===
If you want to put resin back in the bottle from the vat, filter it with a proper filter to avoid hard pieces getting in.
 
Hard flakes from failed prints damage the foil which will need replacing earlier.


== Mechanics of usage ==
== Mechanics of usage ==
Read this before designing any object for printing. Maybe you realize you don't actually want to bother.
Read this before designing any object for printing. Maybe you realize you don't actually want to bother.


=== Preparation ===
You'll need:
 
* toilet paper
* toothbrush
* isopropyl alcohol
 
=== First-time preparation ===


# Unscrew the vat, '''carefully''' slide it out (don't scratch the display underneath)
# Unscrew the vat, '''carefully''' slide it out (don't scratch the display underneath)
# Clean out the remaining resin with a silicon spatula, and by rubbing a piece of cloth soaked in isopropyl alchol (unless you want to re-use the resin).
# Clean out the remaining resin with a silicon spatula, and by rubbing a piece of cloth soaked in isopropyl alchol (unless you want to re-use the resin).
# Use the interface to lift the arm up a lot.
# Use the screen interface to lift the arm up a lot.
# Unscrew the hex bolt on the side of the lifting arm. It should be possible to wobble it without a lot of force.
# Unscrew the hex bolt on the side of the lifting arm. It should be possible to wobble it without a lot of force.
# Use the interface to level the arm: press the "home" icon.
# Use the interface to level the arm: press the "home" icon.
Line 44: Line 69:
# Save the setting in the software.
# Save the setting in the software.
# Fill in the vat with resin. Make sure the '''entire''' bottom is covered, and that there is enough extra resin for the object.
# Fill in the vat with resin. Make sure the '''entire''' bottom is covered, and that there is enough extra resin for the object.
=== Every-time preparation ===
# Take out the vat.
# Wipe any spilled resin off the UV screen.
# Scratch off hardened resin from UV screen '''with a fingernail'''.
# Slush the resin in the vat, look against a light for unevenness floating on the surface. Hard pieces have the same color as the fluid so they are invisible.
# Fish them all out with a toothbrush.
# Slide in the vat, screw it in.
# Slide in the vat, screw it in.
# Close the lid.
# Close the lid.
# Power off the device
# Power off the printer.
# Insert USB stick with the prepared file
# Insert USB stick with the prepared file
# Power on the device
# Power on the device
Line 58: Line 90:
The object will be stuck to the top plate and everything will be sticky with resin.
The object will be stuck to the top plate and everything will be sticky with resin.


# Prepare a toothbrush, toilet paper, and a closeable liquid container big enough to soak your object
# Unscrew the big screw on top of the lifting arm
# Unscrew the big screw on top of the lifting arm
# Slide out the lifting arm
# Slide out the build plate from the arm
# Use a metal scraper (not available, find one) to get your object off the arm plate, and put the object on toilet paper
# Use the knife to gently pry your object off the build plate, and put the object on toilet paper
# Replace the lifting arm and screw it back on.
# Wipe the remaining resin from the build plate.
# Wipe your object with toilet paper
# Replace the build plate and screw it back on.
# Soak the toothbrush in isopropyl alcohol and brush the object
 
# Fill the container with isopropyl alcohol, put your object inside and shake it to dissolve uncured resin (how long?)
=== Finishing the object ===
# Find a sunny place and leave your object there to finish curing with UV light from the Sun (may take many hours, doesn't work at night).
 
# Clean '''all resin residue''', because it will harden with exposure to natural UV light.
==== Excess resin ====
# Don't pour anything into the sewer. Leave the isopropyl alcohol to evaporate in an open container. Whatever liquid resin is left, wait until it cures and then trash it.
If your object has fine details, you want to get rid of excess resin, because it will harden with exposure to natural UV light and take details away.
# If you don't intend to come back within a couple days, then pour resin from the vat back to the bottle (use the paper funnel to filter hardened residue) and clean the vat.
 
===== Toilet paper =====
soak with isopropyl alcohol, wipe. It might be enough.
 
===== Toothbrush =====
soak with isopropyl alcohol, brush. It might be enough.
 
===== Isoprop bath =====
Put object in the jar with isopropyl alcohol, shake for a minute.
 
==== Curing ====


=== Curing ===
* Curing in the sun works well. The print will start curing after seconds in full sun.
There's an experimental curing box with UV light inside. It seems to need several hours to cure unwashed resin. Please write your experiences using it in the paper log.
* There's an experimental curing box with UV light inside. It seems to need several hours to cure unwashed resin. Please write your experiences using it in the paper log.
* There's an experimental nail curing machine. It has no box and switches off after 60s.


Sources say exposure to oxygen prevents curing.
Sources say exposure to oxygen prevents curing.


== Software ==
==== Shiny and translucent objects ====
Objects come out matte after cleaning. Shiny/translucent surfaces take a lot more care.
 
* Remove flakes from the surface. Use cotton swabs if needed to reach difficult spots. Form them into a spike with your fingers if you need to access corners.
* Dip brush in resin, cover the surface with a layer as thin as you can.
* Cure fast! The resin will not stay in place for long.Software
 
The USB stick must be MBR (ms-dos), Fat32 formatted (primary partition).
The USB stick must be MBR (ms-dos), Fat32 formatted (primary partition).



Revision as of 08:34, 7 April 2025

🛸 Location: Chemistry lab

Another 3D printer. It uses liquid resin which gets solidified using UV light rather than solid plastic which gets melted into a new shape. It's slower (each print takes a day or 2), dirtier, and requires more effort, but it promises more detailed objects and translucent objects, compared to the filament printer.

Contents

  • The printer itself: Anycubic Photon Mono SE
  • A curing cookie box with UV light inside
  • A roll of toilet paper
  • A small jar with isopropyl alcohol to wash prints
  • A box with:
    • bottles of resin (grey, transparent)
    • film replacements
    • resin filters
    • vials with extra resin
    • rubber gloves
    • face mask
  • A tray with:
    • a knife to pry prints off the build plate
    • a silicon spatula to stir resin in the vat
    • a syringe to measure resin
    • a brush to spread resin to make prints shiny

Experimental

This printer is currently in the experimental state. Please don't use it without first talking to someone who has some experience.

Precautions

Read this before starting.

Safety

Using the printer involves dangerous chemicals and processes:

  • the resin is a skin irritant - wear gloves and glasses. Always wash your hands after handling objects in the printer station.
  • the resin stinks and can't be healthy - make sure there's enough ventillation (there's a pipe in the wash room)
  • isopropyl alcohol for cleaning is an irritant and stinky
  • the printer emits near-UV light, which leaks outside and damages living organisms - rather be outside the room when it's working
  • drop used toilet paper in the chemical waste bucket on the floor

Cleanliness

Resin is sensitive to sunlight (405nm wavelength) and hardens after a day or so even in the relative dark.

  • Wipe resin from surfaces using toilet paper when you leave the station.
  • Use brown containers to store extra resin
  • After using a brush or syringe or some other tool with resin, wash it well with isopropyl alcohol.

Materials

If you want to put resin back in the bottle from the vat, filter it with a proper filter to avoid hard pieces getting in.

Hard flakes from failed prints damage the foil which will need replacing earlier.

Mechanics of usage

Read this before designing any object for printing. Maybe you realize you don't actually want to bother.

You'll need:

  • toilet paper
  • toothbrush
  • isopropyl alcohol

First-time preparation

  1. Unscrew the vat, carefully slide it out (don't scratch the display underneath)
  2. Clean out the remaining resin with a silicon spatula, and by rubbing a piece of cloth soaked in isopropyl alchol (unless you want to re-use the resin).
  3. Use the screen interface to lift the arm up a lot.
  4. Unscrew the hex bolt on the side of the lifting arm. It should be possible to wobble it without a lot of force.
  5. Use the interface to level the arm: press the "home" icon.
  6. Once the arm is flat on the display, adjust the rotation and repeat leveling if needed
  7. Hold the arm to the display and tighten the screw.
  8. Save the setting in the software.
  9. Fill in the vat with resin. Make sure the entire bottom is covered, and that there is enough extra resin for the object.

Every-time preparation

  1. Take out the vat.
  2. Wipe any spilled resin off the UV screen.
  3. Scratch off hardened resin from UV screen with a fingernail.
  4. Slush the resin in the vat, look against a light for unevenness floating on the surface. Hard pieces have the same color as the fluid so they are invisible.
  5. Fish them all out with a toothbrush.
  6. Slide in the vat, screw it in.
  7. Close the lid.
  8. Power off the printer.
  9. Insert USB stick with the prepared file
  10. Power on the device
  11. Select the file in the interface
  12. Start printing

Printing

Leave the room, leave ventillation on, and come back in a couple hours.

Finishing

The object will be stuck to the top plate and everything will be sticky with resin.

  1. Unscrew the big screw on top of the lifting arm
  2. Slide out the build plate from the arm
  3. Use the knife to gently pry your object off the build plate, and put the object on toilet paper
  4. Wipe the remaining resin from the build plate.
  5. Replace the build plate and screw it back on.

Finishing the object

Excess resin

If your object has fine details, you want to get rid of excess resin, because it will harden with exposure to natural UV light and take details away.

Toilet paper

soak with isopropyl alcohol, wipe. It might be enough.

Toothbrush

soak with isopropyl alcohol, brush. It might be enough.

Isoprop bath

Put object in the jar with isopropyl alcohol, shake for a minute.

Curing

  • Curing in the sun works well. The print will start curing after seconds in full sun.
  • There's an experimental curing box with UV light inside. It seems to need several hours to cure unwashed resin. Please write your experiences using it in the paper log.
  • There's an experimental nail curing machine. It has no box and switches off after 60s.

Sources say exposure to oxygen prevents curing.

Shiny and translucent objects

Objects come out matte after cleaning. Shiny/translucent surfaces take a lot more care.

  • Remove flakes from the surface. Use cotton swabs if needed to reach difficult spots. Form them into a spike with your fingers if you need to access corners.
  • Dip brush in resin, cover the surface with a layer as thin as you can.
  • Cure fast! The resin will not stay in place for long.Software

The USB stick must be MBR (ms-dos), Fat32 formatted (primary partition).

PrusaSlicer can produce files compatible with this printer. Place the resulting file in the root directory of the USB stick.

Random tips

Large objects can be hollowed out by the slicer.

You can print directly on the base if you select "Pad: around object". The first layer will be flatter.

You can save resin on big objects by creating a hollowed-out profile. Wall thickness of 1mm should be enough for more uses.

This is a monochromatic model, meaning it's fast. 1s is enough exposure time for 0.05mm layer height. When it's cold, use 2s.

Translucent objects

They won't shine after cleaning, but rather be cloudy. Internet suggests solutions like varnish, spray, or dipping in resin.

  • Nail polish varnish scratches off easily, smells, and feels slightly rubbery

Problems

The object is stuck to the plate so hard it breaks while scraping

Reduce exposure time for the first layer from 40s to 20s.

No object, only supports on the plate

Slow down retraction, also add more supports and position the object better. More info.

Rationale: the plate pulls the object up and away from the membrane. That's a strong pull (makes noise) and weak or off-center supports may not survive it (pay attention to rotating forces?).

Gaps in object

Increase wait time after dropping and before light on (tested and works).

Rationale: the build plate needs to settle at the minimal penetration height. This takes time because resin is very viscous.

The side attached to the plate is too flat

Use supports and cut them off later. The first layers will be overexposed in order to stick to the plate, and have relatively bad quality.